Correct rendering of major unevennesses
Simple & safe to the goal
-
1. Whenever uneven masonries with variations in render thickness > 5 mm as consequence, work must be carried out in several layers, otherwise stresses will arise within the render layer due to the excessively different thicknesses, which can lead to cracks.
-
2. The first render layer is applied up to 30 mm thick, preferably with the very lightweight lime-cement and fiber-reinforced render weber.dur 140 SLK. After a standing time of 1 day per mm thickness, a 2nd layer of uniform thickness is applied.
Necessary products for this solution
Find all our products near you in more than 2000 outlets